img_wrcobb_banner
Not registered yet? Click here
Yellow Golds
Master Alloy: 2Y9
Color: Yellow
Usage: 22K
Material Characteristics 22K
Density
18.36
Hardness - Cold worked (reduced 60%)
127 Hv
Hardness - Reduced 60%, annealed 15 minutes at 680C, water quenched
<100 Hv
Hardness - Reduced 60%, annealed 15 minutes at 680C, air cooled
<100 Hv
Investment Casting Parameters
Metal Pouring Temperature
1070C
Quench Time
15min