Master Alloy: Y619
Color:
Yellow
Usage:
10K and 14K
Material Characteristics
10K
14K
Density
12.65
14.02
Hardness - Cold worked (reduced 60%)
228 Hv
228 Hv
Hardness - Reduced 60%, annealed 15 minutes at 680C, water quenched
153 Hv
147 Hv
Hardness - Reduced 60%, annealed 15 minutes at 680C, air cooled
180 Hv
117 Hv
Investment Casting Parameters
Metal Pouring Temperature
995C
1010C
Quench Time
20 min.
20 min.